钠离子电池层状氧化物正极:层间滑移,相变与性能
刘欢庆, 高旭, 陈军, 尹首懿, 邹康宇, 徐来强, 邹国强, 侯红帅, 纪效波

Layered oxide cathode for sodium ion batteries: Interlayer glide, phase transition and performance
Huanqing LIU, Xu GAO, Jun CHEN, Shouyi YIN, Kangyu ZOU, Laiqiang XU, Guoqiang ZOU, Hongshuai HOU, Xiaobo JI
图3 (a)(d) NaCrO2NaNiO2O3-NaNi0.5Mn0.5O2 and O3-NaxMn1/3Fe2/3O2的相演化[37, 43, 48](e) 2.04.3 V范围内O3-Na1-δNi1/3Fe1/3Mn1/3O2电极的原位XRD[51](f) NaFe0.2Mn0.4Ni0.4O2电极的非原位XRD[45]
Fig.3 (a)(d) phase evolutions of NaCrO2, NaNiO2, O3-NaNi0.5Mn0.5O2 and O3-NaxMn1/3Fe2/3O2[37, 43, 48]; (e) in-situ XRD patterns collected during cycling of O3-Na1-δNi1/3Fe1/3Mn1/3O2 electrode between 2.0 and 4.3 V[51]; (f) ex-situ XRD pattern of NaFe0.2Mn0.4Ni0.4O2 electrode[45]