钠离子电池层状氧化物正极:层间滑移,相变与性能
刘欢庆, 高旭, 陈军, 尹首懿, 邹康宇, 徐来强, 邹国强, 侯红帅, 纪效波

Layered oxide cathode for sodium ion batteries: Interlayer glide, phase transition and performance
Huanqing LIU, Xu GAO, Jun CHEN, Shouyi YIN, Kangyu ZOU, Laiqiang XU, Guoqiang ZOU, Hongshuai HOU, Xiaobo JI
图6 (a) Na0.7Mg0.05[Mn0.6Ni0.2Mg0.15]O2的原位XRD[77](b) Na2/3Mn1-yMgyO2 (y=0.0, 0.05 and 0.1) 化合物的电化学曲线[46](c) Na0.66Li0.18Fe0.12Mn0.7O2电极中锂的核磁共振谱(NMP[32](d)(e) Zn取代的NaxMnO2电极的原位XRD表征及相应的晶格参数c演变[79]
Fig.6 (a) in-situ XRD patterns of the Na0.7Mg0.05[Mn0.6Ni0.2Mg0.15]O2[77]; (b) electrochemical profiles of the Na2/3Mn1-yMgyO2 (y=0.0, 0.05 and 0.1) compositions[46]; (c) 7Li NMR spectra of Na0.66Li0.18Fe0.12Mn0.7O2 electrode[32]; (d)(e) in-situ XRD characterization and corresponding lattice parameter c evolutions of Zn-Substituted NaxMnO2 electrode[79]