[an error occurred while processing this directive]
助熔剂法制备单晶LiNi0.8Co0.1Mn0.1O2正极材料
任思佳1,2(), 田雷武1,2, 邵钦君1,2, 陈剑1()
Synthesis of single-crystal LiNi0.8Co0.1Mn0.1O2 by flux method
Sijia REN1,2(), Leiwu TIAN1,2, Qinjun SHAO1,2, Jian CHEN1()

图7. 采用(a) NCM-S0和(b) NCM-800-2材料制备的扣式电池的CV曲线,扫描速率为0.10 mV/s

Fig.7. Cyclic voltammetric curves obtained with cells fabricated with (a) NCM-S0 and (b) NCM-800-2 cathodes, respectively. Potential scan rate 0.1 mV/s