采用阳极预锂化技术的锂离子电池高倍率老化容量衰减机理研究
赵鹤1,2(), 韩策1, 程小露1, 郝维健1, 徐涵颖1, 耿萌萌3, 杨凯3, 赵丰刚4, 邱新平1()
Research on the capacity fading mechanism of high rate aged lithium-ion batteries with anode prelithiation treatment
He ZHAO1,2(), Ce HAN1, Xiaolu CHENG1, Weijian HAO1, Hanying XU1, Mengmeng GENG3, Kai YANG3, Fenggang ZHAO4, Xinping QIU1()

图2. 不同放大倍数的PRE电极SEM照片:(a)(b)初始状态负极材料;(c)(d)首次充满电状态正极材料

Fig. 2. SEM images of PRE electrodes at different magnification: (a) and (b) pristine anode; (c) and (d) first charged cathode