锂离子电池富镍三元正极材料NCM的研究进展
张言, 王海, 刘朝孟, 张德柳, 王佳东, 李建中, 高宣雯, 骆文彬

Research progress of nickel-rich ternary cathode material ncm for lithium-ion batteries
ZHANG Yan, WANG Hai, LIU Zhaomeng, ZHANG Deliu, WANG Jiadong, LI Jianzhong, GAO Xuanwen, LUO Wenbin
图5 (a) 不同退火温度下SC-NCM5-ZrO2-NCMZr 3d[44](b) 退火温度对材料性能的影响[45](c) ZrB2 掺杂对NCM811正极循环时机械稳定性的影响示意图[46]