固态锂电池聚合物电解质研究进展
周伟东, 黄秋, 谢晓新, 陈科君, 李薇, 邱介山

Research progress of polymer electrolyte for solid state lithium batteries
ZHOU Weidong, HUANG Qiu, XIE Xiaoxin, CHEN Kejun, LI Wei, QIU Jieshan
表2 PS-SPE的离子电导率及电化学窗口
Table 2 Ionic conductivities and electrochemical windows of PS-SPE
类型聚合物电解质离子电导率/(S/cm)电化学窗口/V文献
接枝VTMS-PMHS/LiPF61.12×10-3 (25 ℃)>4.0[54]
VC-PMHS/PVDF/LiTFSI1.55×10-4 (25 ℃)4.9[55]
ABPTP80/LiTFSI4.0×10-4 (60 ℃)>4.5[56]
交联PSi-S-CN/LiTFSI4.8×10-5 (60 ℃)3.95[57]
CSPE-BFs/LiTFSI1.3×10-4 (60 ℃)5[58]
PSi-g-CN/LiClO4

1.15×10-5 (20 ℃)

1×10-4 (60 ℃)

5[59]
共聚(共混)P(DMS-co-nEO)/LiClO42.6×10-4 (25 ℃)5[60]
D m CS n /LiTFSI1.15×10-4 (25 ℃)4.5[61]
POEM-g-PMDS/LiCF3SO3

9×10-6 (25 ℃)

6×10-5 (60 ℃)

>4[62]