基于三维电化学热耦合析锂模型的锂离子电池参数设计
马勇, 李晓涵, 孙磊, 郭东亮, 杨景刚, 刘建军, 肖鹏, 钱广俊

Parameter design of lithium-ion batteries based on a three-dimensional electrochemical thermal coupling lithium precipitation model
Yong MA, Xiaohan LI, Lei SUN, Dongliang GUO, Jinggang YANG, Jianjun LIU, Peng XIAO, Guangjun QIAN
表3 析锂与可逆锂重嵌入动力学反应相关参数
Table 3 Parameters related to the kinetic reactions of analytical and reversible lithium re-embedding
参数物理意义单位负极
αa, plαc, pl析锂/锂溶解传递系数10.3、0.7[19]
kpl/st锂析出/溶解反应速率常数m/s6.5×10-6
Ea, pl/st析锂与锂溶解反应活化能J/mol50000
z1z2z3可逆锂/不可逆锂/SEI占比10.57、0.375、0.05
σSEISEI膜电导率S/m5×10-6[19]
δSEISEI膜t厚度m式(10)
ρSEISEI 膜密度kg/m31690[19]
ρLi锂金属密度kg/m3534[19]
MSEISEI膜摩尔质量kg/mol0.162[19]
MLi锂金属摩尔质量kg/mol6.94×10-3[19]