表3 三组工况热失控温度与表面最高温度
Table 3 Thermal runaway temperature and maximum surface temperature of 3 cases
序号滥用方式热失控温度Ttr表面最高温度Tmax
1过充(96.5±4.2) ℃(249.1±36.4) ℃
2过热(151.0±8.5) ℃(721.1±21.1) ℃