面向高电压固态锂电池的明胶/聚氧化乙烯复合电解质的制备与性能
郑衍森, 王泳茵, 桂久青, 谢卓豪, 徐越, 曹巧英, 徐悦华, 刘应亮, 梁业如

Preparation and performances of gelatin/polyethylene oxide composite electrolyte for high-voltage solid-state lithium batteries
Yansen ZHENG, Yongyin WANG, Jiuqing GUI, Zhuohao XIE, Yue XU, Qiaoying CAO, Yuehua XU, Yingliang LIU, Yeru LIANG
图6 (a)~(c)Li|PEO|NCM811(d)~(e)Li|G/PEO|NCM811高电压搁置15 h后正极界面组分C1sXPS图谱
Fig. 6 (a)—(c) XPS spectra of positive electrode interface components C1s after high voltage storage for 15 hours for Li|PEO|NCM811 and (d)—(e) Li|G/PEO|NCM811