钠离子电池普鲁士蓝材料结构构建及优化的研究进展 |
陈娜, 李安琪, 郭子祥, 张钰哲, 秦学 |
Research progress on the construction and optimization of Prussian blue material structure for sodium-ion batteries |
Na CHEN, Anqi LI, Zixiang GUO, Yuzhe ZHANG, Xue QIN |
图2 Pb和PbAs骨架的晶体结构示意图,完整A x MA[MB(CN)6] (左) 及理想缺陷的A x MA[MB(CN)6]0.75·? 0.25·nH2O (右) 的晶体骨架,理想缺陷每个晶胞中存在25%Fe(CN)6 空位[ |
Fig. 2 Left: An intact A x MA[MB(CN)6] framework without structural defects, Right: An ideally defective A x MA[MB(CN)6]0.75·? 0.25·nH2O framework with 25% Fe(CN)6 vacancies existing in each unit cell[ |
![]() |