基于SVD-SAE-GPR的锂离子电池RUL预测
|
董渊昌, 庞晓琼, 贾建芳, 史元浩, 温杰, 李笑, 张鑫
|
Remaining useful life prediction of lithium-ion batteries based on SVD-SAE-GPR
|
Yuanchang DONG, Xiaoqiong PANG, Jianfang JIA, Yuanhao SHI, Jie WEN, Xiao LI, Xin ZHANG
|
|
表1 四个电池15个潜在HIs与容量的Spearman相关分析
|
Table 1 Spearman correlation analysis of 15 potential HIs and capacity of four batteries
|
|
特征提取对象 | HIs | Spearman相关系数 |
---|
B0005 | B0006 | B0007 | B0018 |
---|
放电电压 | HI1 | 0.9943 | 0.9982 | 0.9953 | 0.9876 | 放电电流 | HI2 | 0.9873 | 0.9986 | 0.9949 | 0.9888 | 放电温度 | HI3 | 0.8118 | 0.6690 | 0.8864 | 0.9688 | 放电负载电压 | HI4 | 0.9953 | 0.9986 | 0.9945 | 0.9917 | 放电负载电流 | HI5 | 0.9870 | 0.9987 | 0.9945 | 0.9892 | 放电数据测量时间 | HI6 | 0.9972 | 0.9976 | 0.9951 | 0.9929 | 充电电压 | HI7 | -0.3348 | -0.3289 | -0.3518 | 0.9707 | 充电电流 | HI8 | 0.9908 | 0.9908 | 0.9912 | 0.9734 | 充电温度 | HI9 | -0.2286 | -0.2668 | -0.2123 | 0.9567 | 充电负载电压 | HI10 | -0.3144 | -0.3237 | -0.5934 | 0.9634 | 充电负载电流 | HI11 | 0.9908 | 0.9907 | 0.9913 | 0.9734 | 充电数据测量时间 | HI12 | -0.3560 | -0.3241 | -0.3674 | 0.9349 | | HI13 | 0.9975 | 0.9990 | 0.9959 | 0.9949 | | HI14 | -0.5057 | -0.7387 | -0.3497 | 0.6355 | | HI15 | 0.9833 | 0.9871 | 0.9730 | 0.9929 |
|
|
|