图3 LiNi0.8Co0.1Mn0.1O22% PDMS溶液处理的LiNi0.8Co0.1Mn0.1O2 在潮湿环境不同暴露时间的扫描电子显微(Scanning electron microscopySEM)图像 (a)(d)LiNi0.8Co0.1Mn0.1O2 :初始,暴露24 h72 h120 h (e)(h) 2%PDMS溶液处理后:初始,暴露24 h72 h120 h[38]
Fig. 3 SEM images of bare LiNi0.8Co0.1Mn0.1O2 and 2% PDMS solution-processed LiNi0.8Co0.1Mn0.1O2 for different exposure times: (a) fresh, (b) 24 h exposed, (c) 72 h exposed, and (d) 120 h exposed bare LiNi0.8Co0.1Mn0.1O2; (e) fresh, (f) 24 h exposed, (g) 72 h exposed, and (h) 120 h exposed SiMH-LiNi0.8Co0.1Mn0.1O2[38]