表2 相关工作的倍率性能对比
Table 2 Comparison of rate performance of related work
Anodes0.5C/(mAh/g)1C/(mAh/g)2C/(mAh/g)
3D Cu-InLi-Li149.4138.5122.7
3D Cu-LiBi-Li147.7137.9122.9
Cu-Ge@Li[33]13611270
1D@3D-Cu/Sb-Li[34]~135~122~105
Li-3D HCu-Ag[35]138.4124.9107.6
Al-Li[36]146.5137.3121.3
CNT-Li[37]136.3127.9118.1