天然鳞片石墨球化尾料的高性能负极材料制备及储锂特性研究
周向阳, 胡颖杰, 梁家浩, 周其杰, 文康, 陈松, 杨娟, 唐晶晶

Preparation and lithium storage characteristics of high-performance anode materials based on spheroidized tailings of natural flake graphite
Xiangyang ZHOU, Yingjie HU, Jiahao LIANG, Qijie ZHOU, Kang WEN, Song CHEN, Juan YANG, Jingjing TANG
表5 混酸纯化后所得球化微粉的灰分、振实密度、比表面积及粒度
Table 5 Ash content,Tap density, specific surface area and particle size of Purified spheroidized micro powder
Ash/%TAP/(g/cm3)SSA/(m2/g)D50/μm
0.290.46111.735.108