基于高面容量锌溴液流电池的电堆结构及负极材料设计与优化
孙晓云, 王德仁, 孟琳, 任忠山, 李森森

Design and optimization of cell structure and negative electrode materials for high areal capacity zinc-bromine flow batteries
Xiaoyun SUN, Deren WANG, Lin MENG, Zhongshan REN, Sensen LI
表1 GFs的原子浓度以及从高分辨率C1sO1s谱图中获得的功能团的含量
Table 1 The atomic concentration of the GFs and content of functional groups in C1s and O1s spectra
样品原子浓度*C1s (质量分数)/%O1s (质量分数)/%
COC=CC-CC-OC=OCOOHC=OC-OHC-O化学吸附率
*C+O=100 %
PGF95.614.3959.6622.936.942.683.400.221.901.880.39
TGF395.084.9255.8525.146.652.994.450.372.131.800.62
TGF593.186.8253.3425.486.423.674.270.722.862.510.73
TGF789.8010.2045.0528.508.073.314.870.973.312.093.83